Input Parameters

Simulation speed: x

Length of Rod = 80 mm


Diameter of Rod = 6 mm


Thickness = 1.85 mm


Breadth = 4.8 mm


Polar MOI = 1.272e-10 m4


Stress Applied = 10.34 Mpa


Load on Hanger = 0.8 kg


Temperature = 33℃


Modulus of Rigidity = 29.473 GPa




Simulation Note: For ease of visualization, the specimen is shown as a thicker rod in the simulation. In an actual creep test, the specimen is a thin wire (thread-like) of the material under investigation.


Observations
Time (mins) Extension (mm)
0 0.0